If weld repairs are required, the effects of temper embrittlement can be temporarily reversed (de-embrittled) by heating at ______ for 2 hours per inch of thickness and rapidly cooling to room temperature.
If weld repairs are required, the effects of temper embrittlement can be temporarily reversed (the metal can be de-embrittled) by heating at 1150 °F (620 °C) for 2 hr per 1 in. (25 mm) of thickness and rapidly cooling to room temperature