Graphitization can be prevented by using chromium containing low alloys steels for long-term exposure above ________.

  • A. 650º F
  • B. 700º F
  • C. 750º F
  • D. 800º F
Show Suggested Answer Hide Answer
Suggested Answer: D 🗳️

Comments

Chosen Answer:
This is a voting comment (?). It is better to Upvote an existing comment if you don't have anything to add.
Switch to a voting comment New
ahmadmm
1 year, 3 months ago
Graphitization can be prevented by using chromium containing low-alloy steels for long-term operation above 800 °F (425 °C)
upvoted 1 times
...
Community vote distribution
A (35%)
C (25%)
B (20%)
Other
Most Voted
A voting comment increases the vote count for the chosen answer by one.

Upvoting a comment with a selected answer will also increase the vote count towards that answer by one. So if you see a comment that you already agree with, you can upvote it instead of posting a new comment.

SaveCancel
Loading ...
exam
Someone Bought Contributor Access for:
SY0-701
London, 1 minute ago