Thermal fatigue cracks usually initiate on the _________ of the component. They are generally wide and filled with oxides due to the elevated temperatures.
Thermal fatigue cracks usually initiate on the surface of the component, on either the ID or OD surface. They are generally wide and often filled with oxides due to elevated temperature exposure. Cracks may occur as single or multiple cracks.